It is possible I'm being overly literal about the use of words like gold and silver.

http://www.subtleenergies.com/ormus/ormus/ormus2.htm

Here is the basic WET method in brief. It will be discussed later in detail:

1. Start with drinkable water or clean sea water.
2. Slowly add a solution of lye mixed with water to raise the pH above 8.5 but no higher than 10.78.
3. A white fluffy precipitate will form which you should allow to settle overnight.
4. Remove the liquid above the precipitate.
5. Thoroughly wash the precipitate. It is calcium hydroxide, magnesium hydroxide, and a small amount of m-state material.
Here is the DRY method in brief:
1. Start with dry mineral powder.
2. Boil it in lye water at pH 12.
3. Filter and discard the precipitate.
4. Add distilled white vinegar or hydrochloric acid (HCl) to the filtered liquid to lower the pH to 8.5.
5. Let the precipitate settle overnight.
6. Remove the liquid above the precipitate.
7. Wash the precipitate. That is calcium hydroxide, magnesium hydroxide, and a small amount of m-state material.

I can't see myself messing around with hydrochloric acid either.